Parameters | |
---|---|
Package / Case | 100 |
Material | Polyolefin (PO), Chlorinated, Irradiated |
Operating Temperature | -70°C~121°C |
Packaging | Bulk |
Published | 2003 |
Series | HSTTN |
Feature | Abrasion Resistant, Chemical Resistant, Flame Retardant, UV Resistant |
Part Status | Obsolete |
Moisture Sensitivity Level (MSL) | Not Applicable |
Type | Tubing, Flexible |
Max Operating Temperature | 121°C |
Min Operating Temperature | -70°C |
Color | Black |
Shrinkage Ratio | 2 to 1 |
Shrink Temperature | 135°C |
Diameter | 25.4mm |
Diameter - Inner, Supplied | 1.000 (25.40mm) |
Diameter - Inner, Recovered | 0.570 (14.48mm) |
Recovered Wall Thickness | 0.070 1.78mm |
RoHS Status | Non-RoHS Compliant |